[1]卫军,周之津,赵永义,等.实用路面混凝土抗折强度的无损检测方法[J].郑州大学学报(工学版),1992,13(03):31-39.
 Guards,Zhou Zhijin,Zhao Yongyi,et al.Merit and non -destructive detection method of practical pavement concrete folding strength[J].Journal of Zhengzhou University (Engineering Science),1992,13(03):31-39.
点击复制

实用路面混凝土抗折强度的无损检测方法()
分享到:

《郑州大学学报(工学版)》[ISSN:1671-6833/CN:41-1339/T]

卷:
13
期数:
1992年03期
页码:
31-39
栏目:
出版日期:
1992-09-28

文章信息/Info

Title:
Merit and non -destructive detection method of practical pavement concrete folding strength
作者:
卫军;周之津;赵永义;聂建国;
郑州工学院,河南省交通厅公路局,焦作市公路总段,郑州工学院,
Author(s):
Guards; Zhou Zhijin; Zhao Yongyi; Nie Jianguo;
Zhengzhou Institute of Technology, Henan Provincial Department of Transportation Bureau, Jiaozuo City Highway General Section, Zhengzhou Institute of Technology,
关键词:
混凝土抗折强度测试水泥混凝土路面超声回弹综合法
Keywords:
Concrete anti -folding strength test cement concrete pavement ultrasonic rebound comprehensive method
文献标志码:
A
摘要:
通过分析大量试验数据,建立了混凝土抗折强度与超声、回弹测试指标间的相关关系,并详细地研究了现场试验条件对测试结果的影响。制定出一套实用的混凝土强度超声、回弹综合测试方法。经现场实测比较,本方法测试速度快、使用方便,误差在15%以内,能满足工程实用需要。
Abstract:
By analyzing a large amount of test data, the correlation between concrete anti -folding strength and ultrasound and rebound test indicators was established, and the effects of on -site test conditions on the test results were studied in detail. Formulate a set of practical concrete intensity ultrasound and comprehensive test method. After the on -site measurement, the test speed is fast, easy to use, and the error is within 15%, which can meet the practical needs of engineering.

相似文献/References:

[1]王鹏,范磊,崔璨.温度膨胀系数对刚性路面设计的影响分析[J].郑州大学学报(工学版),2014,35(02):6.[doi:10.3969/ j.issn.1671 -6833.2014.02.002]
 WANG Peng,FAN Lei,CUI Can.Effects analysis of CTE on the PCC Pavement Design[J].Journal of Zhengzhou University (Engineering Science),2014,35(03):6.[doi:10.3969/ j.issn.1671 -6833.2014.02.002]
[2]李晶晶,张擎.水泥混凝土路面纵缝拉杆传荷试验研究[J].郑州大学学报(工学版),2015,36(06):119.[doi:10.3969/j. issn.1671 -6833.2015.06.024]
 CHEN Lirong,CHEN Baochun.Analysis of Out-of-plane Stability of Standard Concrete-filledSteel Tube Dumbbell-shaped Rib Arch[J].Journal of Zhengzhou University (Engineering Science),2015,36(03):119.[doi:10.3969/j. issn.1671 -6833.2015.06.024]
[3]廉向东,付欣,熊锐,等.基于层间功能层的水泥混凝土路面动态响应灰关联分析[J].郑州大学学报(工学版),2011,32(06):13.
 LIAN Xiang-dong,FU Xin,XIONG Rui,et al.Grey Incidence Analysis of Dynamic Response of CementConcrete Pavement with Function Layer[J].Journal of Zhengzhou University (Engineering Science),2011,32(03):13.
[4]盛燕萍,李海滨,陈拴发..基于抗冲刷性能的半刚性基层材料组成设计方法[J].郑州大学学报(工学版),2012,33(03):19.[doi:10.3969/j.issn.1671-6833.2012.03.005]
 SHENG Yan-ping,LI Haibin,CHEN Shuanfa.Mix Design of Semi-rigid Base Material Based on Anti-erosion Performance[J].Journal of Zhengzhou University (Engineering Science),2012,33(03):19.[doi:10.3969/j.issn.1671-6833.2012.03.005]
[5]刘文,李清富,胡群芳..水泥混凝土路面结构耐久性设计研究[J].郑州大学学报(工学版),2005,26(04):66.[doi:10.3969/j.issn.1671-6833.2005.04.016]
 LIU Wen,LI Qingfu,Hu Qunfang.Research on durability design of cement concrete pavement structure[J].Journal of Zhengzhou University (Engineering Science),2005,26(03):66.[doi:10.3969/j.issn.1671-6833.2005.04.016]

更新日期/Last Update: 1900-01-01